Eastman SP 2252T EMAC® Ethylene-Methyl Acrylate Copolymer

 

Subcategory: Ethylene Methyl Acrylate; Thermoplastic; Polymer

Key Words: Eastman EMAC

Material Notes:
21% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 350-600°F (177-315°C), Contains a High Level of Slip and Antiblock Additives for Good Surface Characteristics, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability over the Full Processing Temperature Range, Non-Corrosive at Extrusion Temperatures, FDA Clearance for the Packaging of Most Foods, including Aseptic Packaging

Applications:Films: Processable on Standard LDPE Film Lines, Sufficient Melt Strength to Produce 10 mil and Thicker Blown Films, Can be Substituted for PVC Films where Softness and Clean Incineration are Required, Excellent Heat Seal Range, Radio Frequency (RF) Sealable; Compounding: Impact Modification, Compatibilizer; Coextrusion: Excellent Tie Layer for LDPE, HDPE, PET, PP, PVDC, Ionomer, EVA, EAA, rigid PVC, PC; Broad Operating Temperature Range Facilitates Viscosity Matching

Film properties below based on film thickness of 200 µm.

Data provided by Chevron Chemical. Chevron sold its EMAC® and EBAC® product lines to Eastman Chemical in 1999.

Available Properties
  • Density
  • Environmental Stress Crack Resistance
  • Melt Flow
  • Hardness, Shore A
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Elongation at Break
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Coefficient of Friction
  • Dart Drop
  • Melting Point
  • Brittleness Temperature
  • Haze
  • Gloss
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。