Chevron Phillips Chemical Co. Marlex® H516 Polyethylene; HDPE

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Close Analogs: This compound meets or exceeds:

  • ASTM D4976 - PE 235
  • ASTM D3350, class 445574C and 445576C
  • NSF Standards 14 and 61 for potable water
  • PPI designations PE 4710 and PE 100

Material Notes:
High density polyethylene compound. This high performance PE 100 HDPE compound is tailored for the demanding requirements of pressure pipe applications that require:

  • Excellent long-term hoop strength
  • Superb resistance to slow-crack growth
  • Exceptional resistance to rapid-crack propagation
  • Outstanding low-temperature toughness
Additional information: Yellow version also available.

Applications: Typical pipe applications for H516 include:

  • Gas distribution
  • Potable water
  • Industrial applications

Information provided by Phillips

Available Properties
  • Density
  • PENT
  • Melt Flow
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Hydrostatic Design Basis @ 73°F
  • Hydrostatic Design Basis @ 140°F Mpa
  • Hydrostatic Strength, hour
  • Notched Pipe Test @ 4.6 MPa hour
  • Rapid Crack Propagation bar
  • Required Minimum Strength MPa
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。