Solvay Advanced Polymers AMODEL® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, at 50% RH

 

Subcategory: Polyphthalamide; Thermoplastic; Polymer

Close Analogs: This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.

MatWeb has an entry for this material dry as molded.

Material Notes:

Data provided by the manufacturer, Amoco Corporation.

AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is relatively insensitive to moisture which results in good dimensional stability. Therefore, typical humid environmental conditions result in only minor changes in the strength and stiffness. This grade of AMODEL resin can withstand the demanding vapor phase and infrared reflow soldering processes typically used in the electronics industry. It is ideally suited for connectors and electrical devices requiring surface mount technology (SMT). The material offers easy processing using conventional equipment and methods.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。