Solvay Advanced Polymers AMODEL® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded

 

Subcategory: Polyphthalamide; Thermoplastic

Material Notes:
AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properties than many unreinforced thermoplastic polyester and nylon resins especially after exposure to humid environments.

These materials were specifically designed for automotive electrical and electronic applications such as connectors, sockets, and sensors. Additional applications include fuel systems where both the high elongation/ductility and superior low permeation performance to automotive fuels are needed.

They can be processed readily using conventional injection molding equipment and methods.

Information provided by Solvay Advanced Polymers

Available Properties
  • Specific Gravity
  • Moisture Absorption at Equilibrium
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break at Elevated Temperature
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Shear Strength
  • Izod Impact, Notched (ISO)
  • Izod Impact, Unnotched
  • Izod Impact, Unnotched (ISO)
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Dynatup @ -18°C
  • Dynatup @ -18°C Max Load
  • Izod Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Comparative Tracking Index
  • High Voltage Arc-Tracking Rate, HVTR
  • CTE, linear 100°C
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。