Abatron AboCast 50-3/AboCure 50-1 Epoxy

 

Subcategory: Epoxy; Thermoset

Key Words: potting, casting, encapsulating, impregnating

Material Notes:
Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.

Processing: 100/35 ratio. Pot life: 140 min. Peak exothermic temperature is 152°C (306°F). Cures at RT, but full mechanical, thermal, and corrosion properties are developed by heat cure or postcure.

Applications: General purpose for casting, thick coating, bonding, embedding.

Information provided by Abatron, Inc.

Available Properties
  • Viscosity
  • Hardness, Rockwell M
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Yield Strength
  • Compressive Modulus
  • Izod Impact, Notched
  • Electrical Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Maximum Service Temperature, Air
  • Pot Life
  • Exotherm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。