Abatron AboCast 8006-3/AboCast 8606-3 Clear Versatile Epoxy

 

Subcategory: Epoxy; Thermoset

Material Notes:
AboCoat 8006-3/AboCoat 8606-3 is a 2-component clear versatile epoxy for protective and dielectric coatings.

Suggested Uses: Heavy-duty all-purpose protection against water, alkalis, diluted acids, common solvents, corrosion, wear. Corrosion inhibition also on tightly bound rust. Superior salt spray resistance in marine and industrial applications. Concrete, wood and metal floors coating. Brushing on moist or wet surfaces tends to emulsify water, which then evaporates with solvent. Protection of wooden furniture in plants, laboratories, commercial kitchens, hospitals. Most effective for protection of all kinds of electric and electronic components.

Processing:

Ratio by volume: 1 part AboCoat 8006-3 (clear resin in organic solvent) to 1 part AboCoat 8606-3 (clear converter in organic solvent).

Cure Schedule: Room temperature cure 4-6 hours for handling, 3-4 days for full physical properties, and 6-8 days for full chemical properties. High temperature cure 25 minutes at 200°F, 15 minutes at 250°F, 10 minutes at 300°F, or 5 minutes at 350°F.

Information provided by Abatron.

Available Properties
  • Density
  • Solids Content
  • Viscosity Measurement
  • Film Elongation at Break, MD
  • Impact Test
  • Gloss
  • Dry Time
  • Pot Life
  • Shelf Life
  • Adhesion
  • Induction Period
  • Mandrel Flexibility
  • Pencil Hardness
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。