Abatron MasterMold 12-3 Flexible Mold Making Compound

 

Subcategory: Epoxy; Polyurethane, TS; Thermoset

Material Notes:
Master mold 12-3 is formulated for versatility, high elasticity and strength. It is a 2-component polyurethane system and can be easily spread on any model to produce a smooth bubble-free mold surface which captures the finest details. Its elasticity, softness and high tear strength permit easy peeling from intricate and undercut shapes. At the same time, its unique dimensional memory permits casting molds without any exterior support in numerous instances. For example, a mold can be removed from a totally enveloped shape, such as a table leg, by cutting one side with a knife. Then the mold can be held together with rubber bands or simple fasteners for casting.

Processing:

Part A Resin: Blue, no-slump thixotropic paste, 8.6 lbs/gal

Part B Converter: Yellow, no-slump thixotropic paste, 11.2 lbs/gal

Information provided by Abatron.

Available Properties
  • Hardness, Shore A
  • Tensile Strength @ Break
  • Elongation at Break
  • Dry Time
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。