EPI Engineered Polymers EP QS Quick Set Epoxy

 

Subcategory: Epoxy; Adhesive; Thermoset

Material Notes:
EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure times, and excellent adhesion characteristics. EP QS can be used as a surface tolerant primer or as a final coat, and will cure in a variety of harsh situations including high humidity. EP QS can be applied at temperatures ranging from 40° F to 120° F. This environmentally friendly epoxy displays excellent chemical resistance, water insensitivity, and UV resistance. EP QS will provide a glossy smooth finish when fully cured. Aggregate can be broadcast into this self-leveling material to provide a non-skid surface. EP QS emits virtually no odors and can be applied indoors with minimal disturbance contributed to high VOC levels found in most epoxies and polyurethanes.

ApplicationsEP QS adheres well to several substrates including concrete, steel, and wood. Some typical uses include:

  • CHEMICAL RESISTANT SECONDARY CONTAINMENT
  • OFFSHORE PLATFORMS
  • MAINTENANCE FACILITIES
  • PRIMER FOR MOST POLYUREAS/POLYURETHANES
  • USDA AND FDA ACCEPTABLE COATING
  • INDUSTRIAL FLOORING
  • TANK COATING
  • Part of the Amber Chemical Group. Data provided by manufacturer.

    Available Properties
    • Viscosity
    • Hardness, Shore D
    • Tensile Strength, Yield
    • Elongation at Yield
    • Flexural Modulus
    • Flexural Strength
    • Adhesive Bond Strength
    • Taber Abrasion, mg/1000 Cycles
    • Izod Impact, Notched
    • Deflection Temperature at 0.46 MPa (66 psi)
    • Flash Point
    • Cure Time
    • Gel Time
    • Color
    • Resistance to Acetic Acid (100%)
    • Resistance to Acetone
    • Resistance to Ammonium Hydroxide (50%)
    • Resistance to Brake Fluid (310g/l)
    • Resistance to Brine-Saturated H2O
    • Resistance to Gasoline
    • Resistance to H2O
    • Resistance to Hydrochloric Acid (50%)
    • Resistance to MEK
    • Resistance to Methanol
    • Resistance to Muriatic Acid (10%)
    • Resistance to NaCl/H2O (10%)
    • Resistance to Nitric Acid (20%)
    • Resistance to Potassium Hydroxide (10%)
    • Resistance to Potassium Hydroxide (20%)
    • Resistance to Sodium Bicarbonate
    • Resistance to Sodium Hydroxide (50%)
    • Resistance to Sodium Hypochlorite (10%)
    • Resistance to Sugar/H2O
    • Resistance to Sulfuric Acid (>50%)
    • Resistance to Sulfuric Acid (10%)
    • Resistance to Toluene
    • Resistance to Xylene
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。