MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

EPI Engineered Polymers EP 82 Silicone Modified Polyurea, SMP™

 

Subcategory: Silicone; Thermoset

Material Notes:
EP 82, “Powered by Reactamine® Technology”, is a new hydrophobic silicone polyurea. The product is characterized by its low viscosity and ability to readily blend with polyisocyanates. It may be processed to produce elastomers of varying hardness. Water absorption of this product is shown to be five to ten times lower than regular polyureas. These elastomers were subjected to a severe hydrolysis test which involves immersing them in water at 90 °C. for a period of 28 days. A similar test has been used for military applications, where specimens are conditioned for 28 days at 100 °C and 95 % relative humidity, stimulating about 10 years of service at 35 °C. and 95 % relative humidity. The EP 82 shows excellent resistance to oxidizing agents, such as those used to treat swimming pools. Thus, chlorinated water resistance of elastomers produced from EP 82 and isocyanates, are superior to those obtained from a conventional polyurea.

Applications: electrical encapsulation, swimming pool filter end-caps, re-enterable encapsulants, cable splicing, and others where the polyurea is exposed to a hard, moisture laden environment, requiring hydrophobic resins that can provide pli necessary resistance to (i) water ingress, (ii) degradation of physical properties and (iii) corrosion of electrical components.

Part of the Amber Chemical Group. Data provided by manufacturer.

Available Properties
  • Water Absorption
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Yield
  • Tear Strength
  • Taber Abrasion, mg/1000 Cycles
  • Resistance to Chlorinated Water Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。