Material Notes:
EP RAP 45 14 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s, aliphatic polyurea coating that was developed for UV stable (colorfast) polyurea flooring applications. This new generation polyurea displays fast cure times and excellent adhesion characteristics. EP RAP 45 14 was designed to be quick gelling (15 minutes) in order to optimize leveling and wetting properties. EP RAP 45 14 can be spray applied at temperatures ranging from 20ºF to 120ºF. This 100% polyurea elastomer displays excellent chemical resistance, water insensitivity and UV resistance (in any color) at a wide range of temperatures. EP RAP 45 14 will provide a smooth glossy finish when fully cured. An aggregate can be broadcast into this self-leveling material to provide a non-skid surface. EP RAP 45 14 emits virtually no odors and can be applied indoors without high VOC levels contributed to most epoxies and polyurethanes. EP RAP 45 14 meets to USDA and FDA specifications.

Applications:

  • AIRCRAFT HANGAR FLOORS
  • LOW TEMPERATURE EQUIPMENT
  • MAINTENANCE FACILITIES
  • FLOORS REQUIRING UV STABILITY
  • UV-STABLE TOP COAT
  • INDUSTRIAL SHOP FLOORS
  • NON-CONDUCTIVE FLOORING
  • Part of the Amber Chemical Group. Data provided by manufacturer.

    Available Properties
    • Viscosity
    • Hardness, Shore D
    • Tensile Strength, Yield
    • Elongation at Yield
    • Adhesive Bond Strength
    • Tear Strength
    • Taber Abrasion, mg/1000 Cycles
    • Flash Point
    • Cure Time
    • Pot Life
    • Color
    • Flexibility
    • Resistance to 1,1,1-Trichlorethane
    • Resistance to Acetic Acid (100%)
    • Resistance to Acetone
    • Resistance to Ammonium Hydroxide (50%)
    • Resistance to Benzene
    • Resistance to Brine-Saturated H2O
    • Resistance to Chlorinated H2O
    • Resistance to Clorox® (10%) H2O
    • Resistance to Diesel Fuel
    • Resistance to Gasoline
    • Resistance to Gasoline/ 5% Methanol
    • Resistance to Gasoline/5% MTBE
    • Resistance to H2O
    • Resistance to H2O (14 days at 82°C)
    • Resistance to Hydraulic Fluid (oil)
    • Resistance to Hydrochloric Acid (20%)
    • Resistance to Hydrofluoric Acid(10%)
    • Resistance to Isopropyl Alcohol
    • Resistance to Lactic Acid
    • Resistance to MEK
    • Resistance to Methanol
    • Resistance to Methylene Chloride
    • Resistance to Mineral Spirits
    • Resistance to Motor Oil
    • Resistance to MTEB
    • Resistance to Muriatic Acid (10%)
    • Resistance to NaCl/H2O (10%)
    • Resistance to Nitric Acid (20%)
    • Resistance to Phosphoric Acid (10%)
    • Resistance to Phosphoric Acid (50%)
    • Resistance to Potassium Hydroxide (10%)
    • Resistance to Potassium Hydroxide (20%)
    • Resistance to Propylene Carbonate
    • Resistance to Skydrol®
    • Resistance to Sodium Bicarbonate
    • Resistance to Sodium Hydroxide (25%)
    • Resistance to Sodium Hydroxide (50%)
    • Resistance to Sodium Hypochlorite (10%)
    • Resistance to Steric Acid
    • Resistance to Sugar/H2O
    • Resistance to Sulfuric Acid (>50%)
    • Resistance to Sulfuric Acid (10%)
    • Resistance to Toluene
    • Resistance to Trisodium Phosphate
    • Resistance to Vinegar/ H2O (5%)
    • Resistance to Xylene
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。