EPI Engineered Polymers EP Primer 28 Aromatic polyisocyanate Prepolymer

 

Subcategory: Thermoset; Polymer

Material Notes:
EP Primer 28 is a polyisocyanate prepolymer based on diphenylmethane diisocyanate (MDI). As corrosion-resistant primers, coatings based on EP Primer 28 polyisocyanate can be formulated to contain zinc as zinc-rich primers that give galvanic protection. To ensure satisfactory intercoat adhesion, recoating intervals must be determined. The high NCO content of EP Primer 28 also makes it an important curing agent for two-component systems. EP Primer 28 polyisocyanate is an outstanding material for moisture-curing one-component formulations and is highly recommended to prime and seal porous substrates. Clear formulations of this type are effective dust-binding impregnants as well as sealers for cement and other substrates because they can protect the substrate from chemicals, deicing salt, and mineral oils. Coatings based on EP Primer 28 polyisocyanate are also used for mold releasing in the building and construction industries. Because of their good resistance to alkalis, they are suitable adhesion primers for solvent-free coating compositions based on ReactAmine® polyisocyanates, ReactAmine® polyesters, and ReactAmine® polyethers. Appropriate catalysts may be added to coatings formulated with EP Primer 28 to influence the curing reaction rate. EP Primer 28 contains 15.5-17.5% NCO, and its euivalent weight is 255 (avg.).

Part of the Amber Chemical Group. Data provided by manufacturer.

Available Properties
  • Specific Gravity
  • Solids Content
  • Viscosity
  • Flash Point
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。