Advanced Elastomer Systems Santoprene™ TPV 8271-55B100 Thermoplastic Elastomer

 

Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)

Key Words: EU 2003/11/EC; RoHS Compliant; FDA 21 CFR 177.1210; FDA 21 CFR 177.2600; NSF 51; UL QMFZ2; UL QMFZ8

Material Notes:
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/PS blends for applications where hard/soft combinations are required. The raw materials of this grade are listed in FDA regulations 21 CFR 177.1210 (Closures with sealing gaskets for food containers) and 21 CRF 177.2600 (Rubber articles intended for repeated use), or are considered as generally recognized as safe (GRAS). Also, this grade has passed the end use extraction testing required in these specific regulations for aqueous-based foods only, and it complies with the good manufacturing practices required in 21 CFR 110. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.

  • Designed for excellent adhesion onto ABS, PS, PC, PMMA and ASA (cold insert or 2K [two-shot] molding).
  • Recommended for applications requiring superior part surface appearance.
  • Designed for soft touch applications.

Information provided by Advanced Elastomer Systems

Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Tensile Strength @ Break
  • Elongation at Break
  • Compression Set
  • Melt Temperature
  • Mold Temperature
  • Color
  • Form
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。