Advanced Elastomer Systems Vistaflex® 641N Thermoplastic Rubber

 

Subcategory: Elastomer, TPE; Thermoplastic

Close Analogs: This grade is no longer a commercial product

Material Notes:
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.

Key Features: Flex modulus (1% Secant) 7.2 MPa (1050 psi); Vicat softening point, 48°C (118°F); Melt flow rate (230°C [446°F], 2160 g [76 oz], 3.5 g [0.1 oz]/10min); Excellent PE and PP modifier for improved impact and flexibility; Smooth part appearance; Snappy 'rubber band' performance; Approved for food contact; Low rubber gel contact for film applications

Additional processing comments: Cycle times: initial inject 0.5 to 5 sec; secondary inject 1.5 to 10 sec. Initial inject pressure: high; just short of flash. Inject speed: just short of flash.

Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 100% Modulus
  • Flexural Modulus
  • Graves Tear Strength
  • Compression Set
  • Tensile Set
  • Vicat Softening Point
  • Brittleness Temperature
  • Processing Temperature
  • Rear Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。