Asahi Glass Co. Fluon® AH-2000 LM-ETFE, Non-Conductive Type, Fluororesin

 

Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE

Material Notes:
Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive agent or surface treatment that is used at previous system. Excellent adhesiveness of the two-layer system is effected for only one step. Furthermore, the conventional properties such as anti stick, excellent moldability and chemical resistance, are same as conventional fluoro-resin.

Information provided by Asahi Glass Company, Inc.

Available Properties
  • Specific Gravity
  • Melt Flow
  • Tensile Strength at Break
  • Elongation at Break
  • Flexural Modulus
  • Izod Impact, Notched
  • Melting Point
  • Permeation Rate
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。