Akzo Nobel Titanocene Dichloride (TDC) Catalyst

 

Subcategory: Polymer

Material Notes:
Titanocene Dichloride and derivatives are used as hydrogenation catalyst for rubbers, like SBS and SEBS, to improve heat stability and resistance to ozone/oxidation. Titanocene Dichloride can also be used with polymethylaluminoxane as a catalyst for metallocene type olefin polymerizations. Titanocene Dichloride is a useful reagent for a wide variety of synthetic transformations. It can be used with Grignard reagents for the reduction of aryl and vinyl halides; with magnesium for the reduction of organic halides, azo compounds, haloketones, and haloesters; with sodium for the reduction of aliphatic aldehydes, esters, and epoxides; for the reductive decyanation of alkyl nitriles; and the reduction of olefins. Titanocene Dichloride has been used with alkylaluminum compounds for the alkylation of a-olefins and alkynylsilanes. It can be reacted with trimethylaluminum to form Tebbe reagent, which is used to transform a carbonyl into a methylene group. Akzo Nobel can further convert Titanocene Dichloride into derivatives required by the customer, e.g. by substituting the Cl-atoms by other groups or by replacing the cyclopentadienyl rings with substituted cyclopentadienyl rings.

Chemical description: Titanocene dichloride
CAS Number: 1271-19-8
Acronym: TDC

Information provided by Akzo Nobel Polymer Chemicals.

Available Properties
  • Density
  • Molecular Weight
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。