BASF Capron® 5202 HS Blend Nylon 66 (Dry)

 

Subcategory: Nylon; Thermoplastic; Nylon 66

Close Analogs: This product is no longer a part of the BASF NAFTA standard product line.

Material Notes:
Capron 5202 HS Blend is a blended, unfilled, heat stabilized, nylon 6,6, injection molding compound. It is also available in natural and pigmented versions. It combines strength and stiffness as well as excellent chemical resistance. The addition of heat stabilizer system extends the retention of properties at elevated temperatures.

Capron 5202 HS Blend is generally recommended for slightly higher temperature and stiffness requirements, such as engine components, power tool guides, straps and other hardware.

Data provided by Allied Signal.

Processing: Max. water content 0.25%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 280-305 degC (536-581 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF)is recommended, but temperatures of as low as 45 degC (113 degF)and as high as 105 degC (221 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Viscosity Measurement
  • Linear Mold Shrinkage
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Yield Strength
  • Poissons Ratio
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。