BASF Capron® 8351 HS BK-102 Impact Modified Nylon 6 (Dry)

 

Subcategory: Nylon; Thermoplastic; Nylon 6

Close Analogs: This product is no longer a part of the BASF NAFTA standard product line.

Material Notes:
Capron 8351 HS BK-102 is a heat stabilized, pigmented black type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughness combined with a moderate flexibility and faster cycles. Excellent thermal and chemical resistance properties provided by the polyamide backbone. It demonstrates the highest impact performance within the Capron copolymer product line while maintaining an excellent balance of strength and stiffness. Excellent chemical resistance to greases, oils and hydrocarbons.

Capron 8351 HS Bk-102 is generally recommended for applications such as spray gun and power tool handles, trim clips and fasteners, wall anchors and automotive roof clips rack components. ASTM Callout PA263 + PA0220 B32310.

Data provided by Allied Signal.

Processing: Max. water content 0.2%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 240-270 degC (464-518 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of 10-95 degC (50-203 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.

Available Properties
  • Density
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Poissons Ratio
  • Electrical Resistivity
  • CTE, linear 20°C
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Processing Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。