Arkema Lacovyl® S 091 PVC

 

Subcategory: Vinyl; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: Polyvinyl Chloride; Polyvinylchloride

Material Notes:
LACOVYL SO 91 is a vinyl chloride homopolymer produced by a suspension polymerization process.

Characteristics :

  • Viscosity index (ISO 1628-2):96 ml/g,(K value:62). Apparent density (ISO 60):0.56 g/ml.
  • molecular weight specially chosen to obtain good mechanical properties whilst maintaining ease of processing.
  • suitable for dry blend preparation providing a controlled feed to production machines.
  • excellent base color and thermal stability.

Provides finished products with good transparency and free from fish eyes.

* RECOMMENDED APPLICATIONS

  • Extrusion blow molding of bottles with improved mechanical properties (pressure resistance for slightly sparkling drinks, stress cracking resistance for oils, detergents...). LACOVYL SO 91 is also recommended for biaxial orientation processes.
  • Calendering or extrusion of rigid and semi-rigid film and sheet.
  • Extrusion and highly transparent sheets and plates.
  • Extrusion of rigid profiles.
  • Injection molding of high mechanical properties articles.

* EXAMPLES OF APPLICATIONS

PVC-U: - NAKAN RPS 400 M - NAKAN RPX 301 L

ISO data provided by the manufacturer, Arkema.

Available Properties
  • Viscosity Test
  • Transmission, Visible
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。