Arkema Oroglas® V 825 HID Acrylic, UV, Heat Resistant

 

Subcategory: Acrylic; Thermoplastic

Close Analogs:
Arkema, formed in 2004, was formerly Atofina Chemicals and before that Elf Atochem.

Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate

Material Notes:
OROGLAS HID is an acrylic resin formulated to withstand continuous exposure to high intensity discharge ( HID ) sources up to 90°c.

Above 80°c, OROGLAS V 825 HID resin retains its original appearance while other plastics typically used in HID lighting yellow.

OROGLAS V 825 HID is specifically designed to be used at the highest acrylic UL relative thermal index, 90°c.

The excellent balance of mechanical, thermal and optical properties are the same as OROGLAS V 825 T resins.

When applications require stability to intense UV light at temperatures above 80°c, OROGLAS V 825 HID deliver superior long term performance. Typically the most demanding lighting applications use high intensity discharge sources.

OROGLAS V 825 HID can be used in any lighting application. It may be a wise choice for certain compact fluorescent or incandescent fixtures where the lens is close to the lamp.

OROGLAS V 825 HID is recognized under all UL component listings and carries a 90°c RTI, the highest o

Available Properties
  • Density
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Melt Flow
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1000 hours
  • Electrical Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Comparative Tracking Index
  • CTE, linear 20°C
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Transmission, Visible
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。