Biomer® L9000 PLLA Biodegradable Polymer

 

Subcategory: Thermoplastic

Material Notes:
PLLA is a thermoplastic polyester of 2-hydroxy lactate (lactic acid). The formula of the subunit is: -[O-CH(CH3)- CO]-.

PLLA is transparent and its surfaces are suitable for optical purposes. It is waterproof and can be processed as classic thermoplastics. The Biomer formulations Biomer® Lxxx (PLLA) are based on poly-L-lactic acid produced by polymerization of naturally occurring L-lactate. Chemically they are alpha hydroxyl esters. These are prone to hydrolyze (degrade). Hydrolysis is fast in humid conditions at temperatures above the glass transition temperature of 50 to 60°C (c.f. bio-degradation in composts). However hydrolysis also is seen at room temperature, although at very low rates.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Linear Mold Shrinkage
  • Melt Flow
  • Deformation
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • Flexural Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Maximum Service Temperature, Air
  • Vicat Softening Point
  • Minimum Service Temperature, Air
  • Glass Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。