Elastane™ 55D Biocompatible Polyether Urethane

 

Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic

Key Words: The Polymer Technology Group; Polyurethane; TPUR

Material Notes:
Excellent Mechanical Properties; Good Biocompatiblity and Biostability; Hydrolytic Stability; Low Temperature Resistance. Noncytotoxic and nonhemolytic.

Elastane™ polyetherurethane is a high-strength, aromatic thermoplastic with a chemical structure and properties similar to Pellethane® 2363 55D, manufactured by the Dow Chemical Company. For more than 25 years, Pellethane has been used to fabricate a large number of implantable devices, including pacemaker leads and cardiac prosthesis devices such as artificial hearts, heart valves, intraaortic balloons, and ventricular assist devices. The Polymer Technology Group developed Elastane in response to Dow's decision to limit Pellethane's use in cardiac prosthesis devices as well as in all medical devices implanted longer than 30 days.

Elastane™ polyetherurethane is a thermoplastic elastomer formed as the reaction product of a polyol, an aromatic diisocyanate, and a low molecular weight glycol used as a chain extender. Polytetramethylene oxide (PTMO) is reacted in the bulk with aromatic isocyanate, 4,4'-methylene bisphenyl diisocyanate (MDI), and chain extended with 1,4-butanediol.

Elastane can be melt processed by conventional extrusion or injection molding equipment. Rod, pellet, and tubing extruded from Elastane displays an excellent surface finish and low gel content. In addition, these materials are heat-sealable, and easily blended with fillers and post-formed.

Information provided by the manufacturer, Polymer Technology Group.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Flexural Yield Strength
  • Tear Strength
  • Taber Abrasion, mg/1000 Cycles
  • Compression Set
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • CTE, linear 20°C
  • Vicat Softening Point
  • Processing Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。