MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Bionate® Polycarbonate-Urethane (PCU), 55 Shore D

 

Subcategory: Polycarbonate; Polyurethane, TP; Thermoplastic

Key Words: The Polymer Technology Group; Polyurethane; PCU

Material Notes:
Clear to slightly cloudy appearance. Molecular Weight Average (GPC) is 264,000; Molecular Weight Number (GPC) is 81,000. Polydispersity (Mw/Mn) is 3.2. Recommended sterilization method is ethylene oxide. Passes USP XXII Class VI Biological Reaction.

Bionate® PCUs were formerly manufactured under the tradename Corethane® Polycarbonate Urethanes by Corvita Corp. The patented Corethane/Coremer/Corehesive polymers are among the most extensively tested biomaterials yet developed, and they are the first biomedical polyurethanes to be promoted for their biostability. This family of materials achieves oxidative stability through a replacement of susceptible ether groups with carbonate linkages adjacent to hydrocarbon groups. This makes these polymers attractive in applications in which oxidation is a potential mode of degradation, such as in pacemaker leads.

Information provided by The Polymer Technology Group.

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • 100% Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Coefficient of Friction
  • Tear Strength
  • Taber Abrasion, mg/1000 Cycles
  • Compression Set
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • CTE, linear 20°C
  • Vicat Softening Point
  • Processing Temperature
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。