BioSpan® Segmented Polyurethane (SPU)

 

Subcategory: Elastomer, TS; Polyurethane, TS; Thermoset

Key Words: SPU; The Polymer Technology Group; Polyurethane; Elastomer

Material Notes:
Used for many biomedical devices due to its flex-life, biostability, thromboresistance, and processability. Typical weight average MW is 180,000 daltons (ASTM D-3593). BioSpan segmented polyurethane (SPU) is one of a series of specialty polyurethanes offered by The Polymer Technology Group. This first generation elastomer is intended as a direct replacement for Ethicon's Biomer®. It is a sightly translucent, polyetherurethaneurea based on a polytetramethyleneoxide soft segment and an aromatic (essentially MDI-ED) hard segment. It contains a stabilizer package virtually identical to Biomer and a similar viscosity-versus-solids content curve (i.e. solution consistency) in dimethylacetamide (DMAC).

The Polymer technology Group has established a master file for this polymer with the US FDA and is working with a number of industrial and academic research groups to provide a wide range of comparativetest results for inclusion in that master file. BioSpan is normally supplied in solution with DMAC but The Polymer Technology Group has facilities for GMP/cleanroom fabrication and can be supplied in configured form.

Information provided by The Polymer Technology Group.

Available Properties
  • Water Absorption
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • Glass Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。