Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems

 

Subcategory: Polypropylene; Thermoplastic

Material Notes:
Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of the excellent performance characteristics of Beta-PPR RA7050-GN is, for example, a categorized required strength (CRS) of 5 MPa at 70°C and 50 years in comparison to a value of 3.21 MPa for standard PP-R. The color of Beta-PPR RA7050 is steel grey similar to RAL7042.

In general Beta-PPR RA7050-GN is intended to be used in applications for plumbing and heating, such as in-house hot and cold water pipes and fittings, floor and wall heating systems and radiator connections.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Melt Flow
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Notched
  • Surface Resistance
  • CTE, linear 20°C
  • Thermal Conductivity
  • Front Barrel Temperature
  • Die Temperature
  • Melt Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。