Borealis Borcoat™ BB127E Polypropylene Adhesive Powder form for Steel Pipe Coating

 

Subcategory: Polypropylene; Thermoplastic

Material Notes:
Borcoat BB127E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the Top-coat polypropylene coating Borcoat BB108E-1199.

Borcoat BB127E is delivered in powder form and can be applied with an ordinary epoxy powder gun. It has excellent adhesion to fusion bonded epoxy and polypropylene. Furthermore it has superior thermal properties and can be used at operating temperatures within the range of -10°C to 110°C, and up to 140°C for specific offshore projects.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Yield
  • Tensile Modulus
  • Izod Impact, Notched (ISO)
  • Peel Strength
  • Vicat Softening Point
  • Front Barrel Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。