Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding

 

Subcategory: Polypropylene; Thermoplastic

Material Notes:
Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is formulated for high speed injection molding and contains nucleating and release additives.

Borpact SG321MO is designed for thin walled containers, lids and houseware articles requiring flexibility, good contact transparency and high impact strength. Examples include thin wall containers, houseware containers and lids, closures with film hinge, and tubes for cosmetic packaging.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Tensile Modulus
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Notched
  • Impact Test
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Melt Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。