Borealis Borstar® FB4230 LLDPE for Film

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer

Material Notes:
Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar FB4250T exhibits a good balance between dart impact combined with excellent yield and tensile strength and improved stiffness. Its toughness also remains in cold climate conditions. The film has good seal strength, wide sealing window and good hot tack force. In addition to the well know Borstar properties, Borstar FB4250T also give good optical properties.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Water Vapor Transmission
  • Oxygen Transmission Rate
  • Thickness
  • Melt Flow
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Impact
  • Impact Test
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop
  • Melting Point
  • Vicat Softening Point
  • Haze
  • Gloss
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。