Borealis Casico™ FR4805 Non Halogen Flame Retardant Compound for Sheathing Energy Cables

 

Subcategory: Polyolefin; Thermoplastic

Material Notes:
Casico FR4805 is a thermoplastic, non-halogen containing natural jacketing compound. It combines high mechanical strength and toughness with flame retardancy. The composition of Casico FR4805 is based on the elements Carbon, Hydrogen, Oxygen, Silicon, and Calcium. Compounds based on these elements will therefore be the only significant constituents of the combustion fumes. Other elements my be present in concentrations less than 0.1%. Flame retardancy is conferred by an inorganic filler and a novel char forming additive

Casico FR4805 is intended to be used as a 90°C rated jacket for fixed building wires (installation cables) and all types of power cables. This product can be used in areas sensitive to smoke or corrosive and toxic combustion products. The principal feature of this product is the high physical strength and toughness. For small downsized cables the enhanced physical properties compensate for reduced cross sectional area. For most cable constructions Casico FR4805 has sufficient flame retardancy to satisfy single wire vertical burning tests. The product contains a UV stabilization system.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Flexural Modulus
  • Electrical Resistivity
  • Dielectric Strength
  • Oxygen Index
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Head Temperature
  • Avergage Rate of Heat Release, kW/m^2
  • Change of Tensile Properties
  • CO, kg/dm^3
  • CO2, kg/dg^3
  • Corrosivity of Combustion Fumes, uS/cm
  • Heat of Combustion, MJ/dm^3
  • Ignition Time, sec
  • Maximum Rate of Heat Release, kW/m^2
  • Pressure Test at High Temp, %
  • Smoke Obscuration, m^2/dm^3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。