Borealis Daploy™ WB135HMS High Melt Strength Polypropylene for Foam Extrusion

 

Subcategory: Polypropylene; Thermoplastic

Material Notes:
Daploy WB135HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is generally characterized by improved processability in polymer forming technologies where stretching flows occur.

Daploy WB135HMS has been developed for thermoformable, foamed films and sheets, lightweight packaging trays, beakers and containers, microwaveable food packaging, technical foams for automotive applications such as headliners, carpet backing, door liners, parcel shelves, water shields, under-the-hood acoustic panels, cushioning and protective packaging, and thermal and acoustic insulation.

Information provided by the Manufacturer.

Available Properties
  • Melt Flow
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Charpy Impact, Notched
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。