Borealis Low Sulfur™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables

 

Subcategory: Ethylene Vinyl Acetate; Thermoplastic

Material Notes:
Low Sulphur LE0594 is designed for use as a conductor and bonded insulation shield for medium and high voltage cables. LE0594 is a peroxide crosslinkable compound and is specifically intended to meet cable specifications based on crosslinked polyethylene insulations. It lends itself readily to various manufacturing processes including triple extrusion.

Low Sulphur LE0594 is based on an ethylene vinyl acetate copolymer (EVA) and is designed to meet the stringent shrinkback requirements for cables with aluminum conductors. It should not be used on copper conductors.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Tensile Strength @ Yield
  • Elongation at Break
  • Electrical Resistivity
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。