Borealis Polycure™ PC780 Flame Retardant Crosslinking Polyethylene Compound for Low Voltage Insulation

 

Subcategory: Polyethylene; Thermoplastic

Material Notes:
Polycure PC780 is a natural, chemically crosslinking polyethylene compound designed for flame retardant low voltage wire insulation and jacketing. PC780 contains a halogen-based, flame retardant additive package designed to reduce normal PE flame spread characteristics and achieve a VW-1 flame resistant rating on 14 AWG wires and larger.

Polycure PC780 is recommended for use in 600 volt power cable and control cable applications. It is also UL approved in applications with oil and gasoline exposure and is suitable for 90°C service in wet conditions.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Tensile Strength @ Yield
  • Elongation at Break
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor, Low Frequency
  • Oxygen Index
  • Front Barrel Temperature
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。