Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation

 

Subcategory: Polyethylene; Thermoplastic; MDPE

Material Notes:
Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 masterbatch accelerates the moisture-induced crosslinking reaction and imparts track resistance, resistance to degradation by ultraviolet light stability to the final product.

Visico ME4425/LE4462 is designed for use as a track resistant insulation for the outer layer of Spacer Aerial Cables and as insulation for Partial Insulated Cables. Although it has been used alone as insulation for cables rated at voltages as high as 35kV, it is recommended that a conductor shield such as LE540 be used for cables rated at voltages above 12 kV or where required by the applicable electrical code.

Information provided by the Manufacturer.

Available Properties
  • Specific Gravity
  • Hardness, Shore D
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Electrical Resistivity
  • Dielectric Strength
  • Track Resistance
  • Brittleness Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。