BorsodChem ONGRONOX INP 75 D peroxide-type initiator

 

Subcategory: Polymer

Material Notes:
Chemical name: Bis-(3,5,5-trimethyl-hexanoyl)-peroxide, or Di-isononanoyl-peroxide.
Mol.wt: 314.50 g/mol.
Active oxygen content: 5.09 %.
Deflegmation material: isododecane.
Major decomposition products: carbon-dioxide, 3,3,5-trimethyl-hexanoic acid, 2,4,4-trimethyl-pentane, 2,2,4,7,9,9-hexamethyl-decane, 2`,4`,4`-trimethyl-pentil-3,5,5-trimethyl-hexanoate.

Field of application: ONGRONOX INP 75D is an initiator for ethylene, vinyl chloride, vinylidenechloride, vinyl-acetate, acrylates etc. polymerization and copolymerization.

Information provided by BorsodChem Rt.

Available Properties
  • Density
  • Molecular Weight
  • Flash Point
  • Oxygen Index
  • free acid content as isononanoic acid, max, %
  • Hydrolizable chlorine
  • Peroxide, %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。