Shell Carilon® D26CX100 Polyketone, Advanced Extrusion Grade

 

Subcategory: Polyketone; Thermoplastic

Material Notes:
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26CX100 is an extrusion grade with mechanical properties that classify it as an engineering thermoplastic. This grade combines high melt strength and viscosity with high chemical resistance and barrier performance. Moreover, this material exhibits a high impact resistance, both at room temperature and at lower temperatures, and good creep performance. CARILON Polymer D26CX100 can also withstand short-term exposure to elevated temperatures. CARILON Polymer D26CX100 has been designed for demanding extrusion processes. This grade should be considered for liners, pipes and large blow moldings.

Data provided by Shell Chemical.

Available Properties
  • Density
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Melt Flow
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Izod Impact, Notched
  • Izod Impact, Unnotched
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。