Shell Carilon® DB6G6P30 Polyketone, Lubricated, Glass-Reinforced, Injection Molding Grade

 

Subcategory: Polyketone; Thermoplastic; Polymer

Material Notes:
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6P2L10 is a high-performance lubricated injection molding grade with mechanical properties which classify it as an engineering thermoplastic. Designed with demanding tribological applications in mind, such as gears, bearings etc., this exceptional grade offers a high limiting pressure velocity ratio, low coefficient of friction and low wear. These benefits are achieved without sacrificing the toughness, moisture resistance and good fatigue performance which characterize the base polymer. CARILON Polymer DA6P2L10 can withstand short-term exposure to elevated temperatures. Moreover, this polymer exhibits a high resistance to hydrocarbons and other chemicals. CARILON Polymer DA6P2L10 is easy to process on standard injection molding equipment. Cycle times are generally short. Parts show good mold definition and little or no warpage. CARILON Polymers' low moisture sensitivity means that no conditioning of parts before assembly or use is necessary.

Data provided by Shell Chemical.

Available Properties
  • Density
  • Water Absorption
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Izod Impact, Notched
  • Coefficient of Friction
  • Limiting Pressure Velocity
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。