CHOMERICS CHO-SHIELD® 2052 Conductive Coating

 

Subcategory: Acrylic; Thermoset; Polymer

Material Notes:
One-component, CHO-SHIELD conductive acrylic, air-dry coatings are intended for EMI shielding of non-conductive substrates. Filler systems include nickel, silver, silver-copper, or nickel-silver blends.

Information provided by Chomerics

Available Properties
  • Density
  • Solids Content
  • Volatile Organic Compounds (VOC) Content
  • Volatiles
  • Thickness
  • Surface Resistivity per Square
  • Shielding Effectiveness
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dry Time
  • Cure Time
  • Cure Time
  • Shelf Life
  • 1-Methoxy-2-propanol
  • 1-Methoxy-2-propanol acetate wt. % Max
  • Acetone wt. % Max
  • Acrylic Copolymer Proprietary wt. % Max
  • Binder
  • Consistency
  • Corrosion Resistance, final, mohms/sq
  • Corrosion Resistance, Humidity - final, mohms/sq
  • Corrosion Resistance, Humidity - initial, mohms/sq
  • Corrosion Resistance, Salt Fog - final mohms/sq
  • Corrosion Resistance, Salt Fog - initial mohms/sq
  • Filler
  • Methyl Ethyl Ketone wt. %
  • Mix Ratio
  • n-Propyl acetate wt. % Max
  • Physical Form
  • Spraying Viscosity, #2 Zahn Cup, sec
  • Theoretical Coverage ft^2/gal
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。