Colorite Polymers 8088 Non-Phthalate 88 Series Vinyl Compound

 

Subcategory: Vinyl; Thermoplastic

Material Notes:
Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doorway applications, as well as inside refrigerated area separators. In both cases, low temperatures are likely to be encountered. All components that are used in the manufacturing of these compounds are sanctioned by the U.S. Food and Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulation. Also, because they sanctioned by the US Department of Agriculture, they may be used in meat packaging plants and other food handling areas with no risk of contamination from the entry separators.

Information provided by Colorite Polymers.

Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 100% Modulus
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。