CPC - Vycom FLAMETEC™ CLEANROOM PVC-C Sheet Material

 

Subcategory: Vinyl; Thermoplastic

Material Notes:
Cleanroom PVC-C sheet material is designed to be the most economical choice in FM 4910 materials. Compression Polymers Corp's Cleanroom PVC-C has been audited and tested in accordance with the FM 4910 protocol. It meets the test criteria with an FPI of 2 (limit of 6 max) and an SDI of 0.1 ( 0.4 max). PVC-C is FM listed.

FEATURES AND BENEFITS

  • Economics- The most economical sheet available for FM 4910 listed products.
  • Weldability- Easy to fabricate with conventional welding equipment. It is also compatible with Corzan® 4910 CPVC.
  • Strength- Superior physical characteristics to handle structural applications, inserts, machining, etc.
  • Compatibility- Completely compatible with Corzan® 4910 CPVC systems and a broad range of semiconductor chemistry.
  • Fire Safe- Listed in accordance to FM 4910 fire safe materials for clean room construction JI 3010757.
  • Extruded Sheet- Extruded sheet offers the best surface quality and gauge consistency.

Information provided by Compression Polymers Corp - Vycom

Available Properties
  • Density
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • CTE, linear 68°F
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。