CPC - Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)

 

Subcategory: Fluoropolymer; Thermoplastic

Material Notes:
Flametec™ Halar® ECTFE (Ethylene Chlorotrifluoroethylene) is an ultra-pure fluoropolymer that is a tough engineering thermoplastic with a balance of physical and chemical properties that qualify it for high performance service in a wide range of applications. It is mechanically both strong and tough, exhibiting high dielectric strength, and can be used in applications over a broad temperature range. As a fluoropolymer, it is highly resistant to most environmental conditions, including corrosive chemicals and organic solvents, strong acids, alkaline, peroxide and SC1 and SC2 chemistries, and aqueous caustics for handling wet or dry chlorine, bromine, and other halogens.

FEATURES AND BENEFITS

  • Purity- Halar has a very low extractable and leaching levels for the most demanding semiconductor applications.
  • Weldability- Easy to fabricate with conventional welding equipment. Extremely strong welds.
  • Strength- High tensile properties and it is very ductile.
  • Economics- The cost of Halar is easily offset by the expense that would normally be incurred by fire suppression equipment.
  • Fire Safe- Accepted in accordance to FM4910, fire safe materials for clean room construction.
  • Extruded Sheet- Offers the best gauge consistency, surface and tolerances.

Information provided by Compression Polymers Corp - Vycom

Available Properties
  • Density
  • Water Absorption
  • Hardness, Rockwell R
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Taber Abrasion, mg/1000 Cycles
  • Izod Impact, Notched
  • CTE, linear 68°F
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Oxygen Index
  • Biofilm Buildup
  • Factory Mutual
  • Mean Roughness
  • Notch Sensitivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。