CPC - Vycom FLAMETEC™ KYTEC® PVDF

 

Subcategory: Vinyl; Thermoplastic; PVDF

Material Notes:
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when exposed to harsh thermal, chemical, and ultraviolet environments. Kytec has a continuous use temperature of 235º F. Kytec is chemically resistant to most acids, bases, and organic solvents and is ideally suited for handling wet or dry chlorine, bromine and other halogens.

FEATURES AND BENEFITS

  • Weldability- Easy to fabricate and thermoplastically weldable.
  • Strength- Good tensile strength and mechanical abrasion resistance.
  • Purity- An ultra-pure material.
  • Chemical Resistance- Resistance to a broad range of chemistries.
  • Fire Safe- Meets FM4910 criteria and is FM listed.

Information provided by Compression Polymers Corp - Vycom

Available Properties
  • Density
  • Water Absorption
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Compressive Strength
  • Izod Impact, Unnotched
  • Coefficient of Friction
  • Coefficient of Friction, Static
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Arc Resistance
  • CTE, linear 68°F
  • Thermal Conductivity
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Brittleness Temperature
  • Oxygen Index
  • Factory Mutual
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。