CPC - Vycom HITEC® HDPE High Density Polyethylene

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Material Notes:
Hitec HDPE is a high impact, high density polyethylene sheet. It is ideally suited for the manufacture of chemical resistant products which come in direct contact with foodstuffs. Hitec meets the standard established by Food and Drug Regulation 21 CFR 177.52 for all food contact, USDA, and the Department of Canadian Agriculture.

FEATURES AND BENEFITS

  • Hardness- Hitec is abrasion resistant and will resist scratching.
  • Strength- Hitec has high tensile and stiffness for machine parts and tank applications.
  • Ductility- Hitec is stress crack resistant.
  • Machinable- Hitec is easy to machine with conventional tools.
  • NSF- The National Sanitation Foundation has approved natural Hitec for food grade contact in food equipment.

Information provided by Compression Polymers Corp - Vycom

Available Properties
  • Density
  • Environmental Stress Crack Resistance
  • Melt Index of Compound
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Modulus
  • Tensile Impact
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。