CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Material Notes:
Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III weather resistant black and ASTM 3350 cell class 345464C.

FEATURES AND BENEFITS

  • Hardness- Hitec Pipe Grade is abrasion resistant and will resist scratching.
  • Strength- Hitec Pipe Grade has high tensile and stiffness for machine parts and tank applications.
  • Ductility- Hitec Pipe Grade is stress crack resistant.
  • Machinable- Hitec Pipe Grade is easy to machine with conventional tools.

Information provided by Compression Polymers Corp - Vycom

Available Properties
  • Density
  • Environmental Stress Crack Resistance
  • ESCR 100% Igepal®
  • Hardness, Rockwell L
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Modulus
  • 2% Secant Modulus
  • Izod Impact, Notched
  • Hydrostatic Design Basis @ 73°F
  • CTE, linear 68°F
  • Melting Point
  • Vicat Softening Point
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。