Cyro Cyrex® 200-8005 Acrylic-Polycarbonate Alloy

 

Subcategory: Polycarbonate; Acrylic; Thermoplastic

Material Notes:
CYREX 200-8005 alloy was formulated specifically for the medical industry. It exhibits excellent resistance to both alcohol and lipids, it has good heat resistance so it can be ethylene oxide sterilized, and it is both gamma and E-beam radiation resistant.

Information provided by Cyro Industries

Available Properties
  • Specific Gravity
  • Water Absorption
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Rockwell M
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • CTE, linear, 212°F (100°C)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Chemical Resistance to Acetone
  • Chemical Resistance to Ammonia
  • Chemical Resistance to Antifreeze
  • Chemical Resistance to Baking Soda Paste
  • Chemical Resistance to Bleach 10%
  • Chemical Resistance to Butter
  • Chemical Resistance to Citric Acid Solution (0.1%)
  • Chemical Resistance to Coffee
  • Chemical Resistance to Diesel Fuel
  • Chemical Resistance to DOP (Phthalate)
  • Chemical Resistance to Ethanol
  • Chemical Resistance to Ethylene Glycol
  • Chemical Resistance to Fantastic Cleaner
  • Chemical Resistance to Fluorides
  • Chemical Resistance to Frenchs Mustard
  • Chemical Resistance to Gasoline
  • Chemical Resistance to Glycerin
  • Chemical Resistance to Heavy Duty Detergent
  • Chemical Resistance to Heptane
  • Chemical Resistance to Igepal (1%) Solution
  • Chemical Resistance to IPA
  • Chemical Resistance to IPA/Water 50%
  • Chemical Resistance to Kerosene
  • Chemical Resistance to Lipids
  • Chemical Resistance to Lipstick
  • Chemical Resistance to Octane/Toluene 75%/25%
  • Chemical Resistance to Rust Inhibitor Veto #4224
  • Chemical Resistance to Rust Inhibitor Veto #53359
  • Chemical Resistance to Soap and Water
  • Chemical Resistance to Sodium Hydroxide (0.5%)
  • Chemical Resistance to Tea
  • Chemical Resistance to Toothpaste
  • Chemical Resistance to Transmission Fluid
  • Chemical Resistance to Vinyl Gasket
  • Resistance to Palmolive Dishwasher/Water 50%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。