Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film

 

Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer

Key Words: FDA: 21 CFR 177.1520 (C) 2.1

Material Notes:
The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product can be easily welded, which is fundamental to satisfy the requirements of cutting, welding and/or bagging lines. The product characteristics allow for a high versatility and use in various applications due to its easy processing and high compatibility with other types of polyethylene. Trithene® TX 7003 resin shows excellent performance with conventional extruders and low energy consumption during processing, which allows producing packaging with dimensional uniformity and excellent surface finishing. This product complies with ASTM standard D1248-IA5 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Heavy duty bags, shrink film and agricultural film. Technical films for high-strength industrial packaging, waterproofing films. Blow-molded bottles with higher stress cracking resistance - ESCR. Blends with HDPE and LLDPE for extrusion and molding processes.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Available Properties
  • Density
  • Thickness
  • Melt Index of Compound
  • Tensile Strength at Break
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Tensile Strength, Yield
  • Elongation at Break
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Coefficient of Friction
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop Test
  • Vicat Softening Point
  • Processing Temperature
  • Feed Temperature
  • Adapter Temperature
  • Blow-up Ratio (BUR)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。