MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; LDPE; Polymer

Key Words: FDA: 21 CFR 177.1520 (C) 2.1

Material Notes:
The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of automatic packaging. The formula developed confers to the Trithene® TS 4016 resin easy processability with conventional LDPE extruders, ensuring films with good appearance, thickness uniformity, and excellent weldability. Furthermore, the incorporated additive package brings thermal stability and good slip performance, which are fundamental for offering high productivity rates on the packaging line. The components that form the product Trithene® TS 4016 complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Technical films for the automatic packaging of food products in the form of grains, powder, or farinaceous, such as cereals, sugar, salt, and flours.

Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Available Properties
  • Density
  • Thickness
  • Melt Index of Compound
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Coefficient of Friction
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop Test
  • Haze
  • Gloss
  • Processing Temperature
  • Feed Temperature
  • Adapter Temperature
  • Proportion LLDPE %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。