Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer

 

Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer

Key Words: FDA: 21 CFR 177.1350

Material Notes:
The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high toughness, and excellent optical properties. These packages may be produced by coextrusion and/or lamination in combination with many others materials as PVdC, PA, EVOH, etc. The resin has flexibility at low temperature that enhances applications in frozen food bags. Additionally, this resin is designed to provide a low temperature heat seal to itself or many other structure and composition commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on blow film equipments over a wide range of film thickness and blow-up ratios. Tritheva TN 8093 can be use as base polymer for the manufacture of film for greenhouses and both large and small tunnels, with excellent thermal effect at low thicknesses. More detailed information about agricultural film applications and light stabilization recommended, please contact Petroquímica Triunfo representative. This product complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1350, to contact with foodstuff.

Applications: Food packaging (meat, cheese), coextruded heat seal layer in food packaging. High clarity film. Base polymer for agricultural film (greenhouse). Stretch hood film.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Available Properties
  • Density
  • Vinyl Acetate Content
  • Thickness
  • Melt Index of Compound
  • Tensile Strength at Break
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Tensile Strength, Yield
  • Elongation at Break
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop Test
  • Melting Point
  • Haze
  • Gloss
  • Processing Temperature
  • Feed Temperature
  • Adapter Temperature
  • Blow-up Ratio (BUR)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。