Dow STYRON™ A-TECH™ 6079 Ignition Resistant Polystyrene Resin

 

Subcategory: Polystyrene; Thermoplastic

Material Notes:
STYRON™ A-TECH™ 6079 is an ignition resistant polystyrene (IRPS) resin designed specifically for consumer and business electronics applications that demand excellent aesthetics, along with a strong blend of toughness and flow/process-ability characteristics. Its high melt flow enables faster cycle times and better flow molding, which reduces scrap/waste. In addition, the molder has a wider operating window with the parameters for larger tools. Available in five colors: Natural, Light Gray, Gray #5, Gray, and Black.

Applications

  • Consumer electronics: larger size TV cabinets
  • Large and/or hard-to-fill parts (including no-paint)
  • Small portable electronics: cellular phones, pagers, etc.
  • Information technology/business equipment: hard drives, monitors, keyboards, printers, fax machine housing, etc.

Information provided by Dow

Available Properties
  • Specific Gravity
  • Melt Flow
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Notched
  • Vicat Softening Point
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。