Dow Plastics UNIVAL™ DMDF-6200 NT 7 High Density Polyethylene Resin (HDPE)

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Material Notes:

  • Excellent extrusion characteristics
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a
UNIVAL™ DMDF-6200 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to produce containers up to 5 gallons in size. This resin is a multipurpose blow molding resin for use in containers that package household industrial chemicals, toiletries and cosmetics, health and medicinal aids, and food products. In addition, it can be blow molded into other thin walled parts and houseware items, and also can be extruded into profiles or sheets.

Information provided by Dow

Available Properties
  • Density
  • ESCR 100% Igepal®
  • Melt Flow
  • Melt Index of Compound
  • Hardness, Shore D
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Tensile Impact Strength
  • Melting Point
  • Crystallization Temperature
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。