DuPont Hytrel® HTR5612 BK320 TPC-ET

 

Subcategory: Polyester, TP; Elastomer, TPE; Thermoplastic

Material Notes:
Hytrel® HTR5612 BK320 is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 50D, is pigmented black with fine particle size carbon black, and contains a general purpose stabilizer.

Available Properties
  • Density
  • Specific Gravity
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Izod Impact, Notched (ISO)
  • Izod Impact, Notched, Low Temp (ISO)
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Notched
  • Izod Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Comparative Tracking Index
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Brittleness Temperature
  • UL RTI, Electrical
  • UL RTI, Mechanical with Impact
  • UL RTI, Mechanical without Impact
  • Flammability, UL94
  • Oxygen Index
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Moisture Content
  • Additive
  • Appearance
  • Drying
  • DuPont Product Category
  • Features
  • Form
  • Part Marking Code
  • Processing Method
  • Region
  • Resin Identification
  • Uses
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。