DuPont Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating

 

Subcategory: Ionomer; Thermoplastic; Polymer

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer

Material Notes:
Surlyn® 1802 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Meat, poultry, seafood and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and nonfood pouches; Carded display/skin packaging films; Edible oil, motor oil, and other liquid product pouches; Snack structures

Data provided by the manufacturer, DuPont Packaging.

Available Properties
  • Density
  • Melt Flow
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Impact
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop
  • Seal Strength
  • Hot Tack Strength
  • Melting Point
  • Vicat Softening Point
  • Haze
  • Gloss
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。